· Japanese· Korean· English

b3

High alumina brick

Высокоглиноземистый кирпич

SK36 Огнеупорный кирпич

Low creep high alumina brick

Fireclay brick
Шамотный кирпич

Fireclay mortar

SK34 Огнеупорный кирпич

Checker fireclay brick

Silica brick

Динас для коксовой печи

Динас для стекловаренной печи

Silica mortar for coke oven

Alkali-resistant Briks

Spinel brick

Магнезитовый кирпич

Магнезитохромитовый кирпич

Carbon Bricks

Firebrick

Carbon block

Silicon carbide brick

Alumina carbon brick

 

  Spinel brick for rotary kiln

    Spinel brick is mainly used in burning zone, transitional zone and kiln mouth of rotary kiln. In particular,spinel brick has been becoming one of the major lining materials for rotary kiln. Spinel brick is applied in the transitional zone, cooling zone, kiln mouth and even in burning zone of ceramic kiln. Spinel brick is replacing magnesium chrome brick step by step. The thermal shock resistance of alkalescency refractory material is poor. The key point of using alkalescency refractory material is that a coating can be formed on surface of kiln. The shortcoming of poor thermal shock resistance can be made up by keeping the proper thickness of coating on kiln(That is 200 to 300mm )Its also applied for spinel brick when it is used in burning zone of kiln.

Index

Fued synthetic Spinel bricks

 sintering synthetic Spinel bricks

MgO/%≥

>78

>80

Al2O3/%≤

10~13

8~12

Fe2O3/%

<1

<1

SiO2/%

<1.8

<1.5

volume density /kg.m-3

≥2920

2920~2950

Apparent porosity %≤

≤19

17~19

Compress strength /MPa≥

≥40

≥40

refractoriness under load   , ℃≥               T0.6 
           T2

≥1650
≥1700

≥1650
≥1700

Linear expansivity  /% (1000℃)

0.96

0.99

thermal conductivity  /W • (m • K ) -1

3.00

3.00

Thermal shock resistance         
(1100℃-Water cold)

≥8

≥8

Spinel brick packing
Products are packed on wooden pallet and then polyethylene film is placed over it, finally the package is tied up with steel strips.
Spinel brick minimum order
20 t of spinal brick can be accepted is our minimum order but more then 2500 t can be supplied per month
Spinel brick delivery time
The delivery time will be 40 days after receiving L/C at sight.

Links:  Oreworld           CSA цемент           Изолируя кирпич 

Oreworld trade (Tangshan) co., Ltd
Fax:0086-315-539-2225
Email:info@oreworld.com